Deformation and Fracture Mechanics of Engineering MaterialsThis Third Edition of the well-received engineering materials book has been completely updated, and now contains over 1,100 citations. Thorough enough to serve as a text, and up-to-date enough to serve as a reference. There is a new chapter on strengthening mechanisms in metals, new sections on composites and on superlattice dislocations, expanded treatment of cast and powder-produced conventional alloys, plastics, quantitative fractography, JIC and KIEAC test procedures, fatigue, and failure analysis. Includes examples and case histories. |
From inside the book
Results 1-3 of 90
Page 18
... material to further plastic deformation — a process known as strain hardening . The portion of the true stress - strain curve ( from the onset of yielding to the maximum load ) may be described empirically by the relationship generally ...
... material to further plastic deformation — a process known as strain hardening . The portion of the true stress - strain curve ( from the onset of yielding to the maximum load ) may be described empirically by the relationship generally ...
Page 41
... material , some additional discussion is indicated . It is known that the general flow curve for a given material will decrease with increasing temperature T and decreasing strain rate è ( Fig . 1.24 ) . The magnitude of these changes ...
... material , some additional discussion is indicated . It is known that the general flow curve for a given material will decrease with increasing temperature T and decreasing strain rate è ( Fig . 1.24 ) . The magnitude of these changes ...
Page 248
... material may exhibit . From theory of plasticity considerations , it is shown that the net section stress in a deformable material may be elevated to 2 to 3 times the smooth bar yield- strength value . It would appear , then , that the ...
... material may exhibit . From theory of plasticity considerations , it is shown that the net section stress in a deformable material may be elevated to 2 to 3 times the smooth bar yield- strength value . It would appear , then , that the ...
Common terms and phrases
alloy aluminum alloy applied stress associated ASTM ASTM STP atom behavior brittle Burgers vector ceramics Chapter Charpy component composite corrosion crack growth rate crack length crack tip craze creep crystal cycles cyclic da/dN decrease depends ductility elastic embrittlement engineering failure fiber FIGURE flaw fracture mechanics fracture surface fracture toughness given grain boundaries hardening hydrogen increasing KIEAC Kmax ksi Vin lattice load martensite material matrix Mech metallurgical microstructure modulus MPaVm Note occur orientation particles phase plane-strain plastic deformation plastic zone plate polymer R. W. Hertzberg ratio region relation relative Reprinted with permission response result rupture sample screw dislocation Section shear stress shown in Fig slip plane slip systems solution specimen stacking fault energy steel alloys strain rate stress concentration stress field stress intensity factor stress level stress-strain curve striation superalloys thickness Trans transition temperature twin values yield strength