Materials Selection for Process Plants |
From inside the book
Results 1-3 of 34
Page 173
Monel ” is widely used in all sorts of waters — fresh , brackish , salt , and high
purity . The rate of attack is negligible under normal service conditions ; even in
services involving slightly elevated temperatures , high flow rates and
considerable ...
Monel ” is widely used in all sorts of waters — fresh , brackish , salt , and high
purity . The rate of attack is negligible under normal service conditions ; even in
services involving slightly elevated temperatures , high flow rates and
considerable ...
Page 174
Although temperature has only a minor effect on the action of sulfuric acid upon “
Monel ” , aeration causes a considerable increase in corrosion . Hot aerated
sulfuric acid solutions are the most aggressive . The steel and heat - treating ...
Although temperature has only a minor effect on the action of sulfuric acid upon “
Monel ” , aeration causes a considerable increase in corrosion . Hot aerated
sulfuric acid solutions are the most aggressive . The steel and heat - treating ...
Page 176
Like " Monel ” , this nickel - chromium - iron alloy has excellent resistance to
attack by all kinds of water ; natural waters rich in free carbon dioxide , chlorides ,
iron compounds , and dissolved air have little effect . “ Inconel ” also is relatively ...
Like " Monel ” , this nickel - chromium - iron alloy has excellent resistance to
attack by all kinds of water ; natural waters rich in free carbon dioxide , chlorides ,
iron compounds , and dissolved air have little effect . “ Inconel ” also is relatively ...
What people are saying - Write a review
We haven't found any reviews in the usual places.
Contents
INTRODUCTION | 1 |
CATHODIC PROTECTION | 23 |
IRON AND STEEL | 44 |
Copyright | |
4 other sections not shown
Other editions - View all
Common terms and phrases
abrasion acid addition alkalies alloys aluminum annealed anode applications atmospheres attack austenitic base brasses carbon carbon steel cast iron cause cements cent characteristics chemical resistance chloride cleaning coat combination common COMPANY compounds concentrations conductivity construction containing continuous cooling copper corrosion corrosion resistance cost cracking ductility effect electrical elevated Elongation environments equipment excellent exposure fabrication film given grades gray greater handled hardness heat heat-treatment improved increase industries lead limited lining lower machining material maximum mechanical properties metal method Monel natural nickel nitric normally occurs operating organic oxidizing paint performed physical pipe plastic prevent protection range readily recommended reducing removed rubber salts silicon sodium hypochlorite solutions solvents stainless steels stress structure suitable sulfuric acid superior surface Table temperature tensile strength thermal thickness tion titanium Type Typical welding widely wrought zinc