GalvanIC SERIES OF METALS AND ALLOYS * Corroded End ( Anodic or Least
Noble ) Magnesium Magnesium alloys Zinc Aluminum Aluminum alloys
Cadmium Carbon steel Cast iron Stainless steel Type 410 ( active ) Stainless
steel Type ...
GalvanIC SERIES OF METALS AND ALLOYS * Corroded End ( Anodic or Least
Noble ) Magnesium Magnesium alloys Zinc Aluminum Aluminum alloys
Cadmium Carbon steel Cast iron Stainless steel Type 410 ( active ) Stainless
steel Type ...
Page 97
All austenitic stainless steels have excellent resistance to nitric acid in all
concentrations and at all temperatures . Most nitric acid plants are fabricated from
Type 304 stainless steel . These steels also finds application in the production
and ...
All austenitic stainless steels have excellent resistance to nitric acid in all
concentrations and at all temperatures . Most nitric acid plants are fabricated from
Type 304 stainless steel . These steels also finds application in the production
and ...
Page 98
Types 321 , 347 , and 348 are stabilized versions of Type 304 . Type 321
contains titanium ; Type 347 contains a mixture of columbium and tantalum . Type
348 is identical to Type 347 , but with a limit on the tantalum content . The
addition ...
Types 321 , 347 , and 348 are stabilized versions of Type 304 . Type 321
contains titanium ; Type 347 contains a mixture of columbium and tantalum . Type
348 is identical to Type 347 , but with a limit on the tantalum content . The
addition ...
What people are saying - Write a review
We haven't found any reviews in the usual places.
Contents
INTRODUCTION | 1 |
CATHODIC PROTECTION | 23 |
IRON AND STEEL | 44 |
Copyright | |
4 other sections not shown
Other editions - View all
Common terms and phrases
abrasion acid addition alkalies alloys aluminum annealed anode applications atmospheres attack austenitic base brasses carbon carbon steel cast iron cause cements cent characteristics chemical resistance chloride cleaning coat combination common COMPANY compounds concentrations conductivity construction containing continuous cooling copper corrosion corrosion resistance cost cracking ductility effect electrical elevated Elongation environments equipment excellent exposure fabrication film given grades gray greater handled hardness heat heat-treatment improved increase industries lead limited lining lower machining material maximum mechanical properties metal method Monel natural nickel nitric normally occurs operating organic oxidizing paint performed physical pipe plastic prevent protection range readily recommended reducing removed rubber salts silicon sodium hypochlorite solutions solvents stainless steels stress structure suitable sulfuric acid superior surface Table temperature tensile strength thermal thickness tion titanium Type Typical welding widely wrought zinc