plastic is insoluble in most solvents and organic chemicals . The common fatty
acids , mineral oils , vegetable oils , and greases have no damaging effect . The
aromatics , ketones , and chlorinated hydrocarbons promote swelling at room ...
plastic is insoluble in most solvents and organic chemicals . The common fatty
acids , mineral oils , vegetable oils , and greases have no damaging effect . The
aromatics , ketones , and chlorinated hydrocarbons promote swelling at room ...
Page 272
Most solvents and many organic chemicals soften the film . The resistance ... To
make a proper coating , the resin plus chlorinated plasticizer is dissolved in
aromatic solvents . Thus , the straight chlorinated rubbers dry by solvent
evaporation .
Most solvents and many organic chemicals soften the film . The resistance ... To
make a proper coating , the resin plus chlorinated plasticizer is dissolved in
aromatic solvents . Thus , the straight chlorinated rubbers dry by solvent
evaporation .
Page 283
The material contains no solvent and , therefore , has no true drying time but sets
as soon as it cools . The cold film has a ... The aliphatic solvents induce some
softening , and aromatic solvents dissolve and destroy the film . Thus , the coal tar
...
The material contains no solvent and , therefore , has no true drying time but sets
as soon as it cools . The cold film has a ... The aliphatic solvents induce some
softening , and aromatic solvents dissolve and destroy the film . Thus , the coal tar
...
What people are saying - Write a review
We haven't found any reviews in the usual places.
Contents
INTRODUCTION | 1 |
CATHODIC PROTECTION | 23 |
IRON AND STEEL | 44 |
Copyright | |
4 other sections not shown
Other editions - View all
Common terms and phrases
abrasion acid addition alkalies alloys aluminum annealed anode applications atmospheres attack austenitic base brasses carbon carbon steel cast iron cause cements cent characteristics chemical resistance chloride cleaning coat combination common COMPANY compounds concentrations conductivity construction containing continuous cooling copper corrosion corrosion resistance cost cracking ductility effect electrical elevated Elongation environments equipment excellent exposure fabrication film given grades gray greater handled hardness heat heat-treatment improved increase industries lead limited lining lower machining material maximum mechanical properties metal method Monel natural nickel nitric normally occurs operating organic oxidizing paint performed physical pipe plastic prevent protection range readily recommended reducing removed rubber salts silicon sodium hypochlorite solutions solvents stainless steels stress structure suitable sulfuric acid superior surface Table temperature tensile strength thermal thickness tion titanium Type Typical welding widely wrought zinc