Deformation and Fracture Mechanics of Engineering MaterialsUpdated to reflect recent developments in our understanding of deformation and fracture processes in structural materials. This completely revised reference includes new sections on isostress analysis, modulus of rupture, creep fracture micromechanicsms, and many more. |
From inside the book
Results 1-3 of 85
Page xxiii
... Fracture - Mode Transition : Plane Stress versus Plane Strain 342 Plane - Strain Fracture - Toughness Testing 337 345 8.8 Fracture Toughness of Engineering Alloys 351 8.9 Plane - Stress Fracture - Toughness Testing 354 8.10 Toughness ...
... Fracture - Mode Transition : Plane Stress versus Plane Strain 342 Plane - Strain Fracture - Toughness Testing 337 345 8.8 Fracture Toughness of Engineering Alloys 351 8.9 Plane - Stress Fracture - Toughness Testing 354 8.10 Toughness ...
Page 406
... fracture based on fundamental engineering properties , such as yield and tensile strength and tensile ductility . Recall from Chapter 1 that toughness was defined by the area under the stress - strain curve ; consequently , toughness ...
... fracture based on fundamental engineering properties , such as yield and tensile strength and tensile ductility . Recall from Chapter 1 that toughness was defined by the area under the stress - strain curve ; consequently , toughness ...
Page 416
... toughness values may be expected to vary with the type of specimen used to measure K , or Kic . This is not related to the specimen shape per ... Fracture - Toughness Anisotropy in. 416 CHAPTER 10 MICROSTRUCTURAL ASPECTS OF FRACTURE ...
... toughness values may be expected to vary with the type of specimen used to measure K , or Kic . This is not related to the specimen shape per ... Fracture - Toughness Anisotropy in. 416 CHAPTER 10 MICROSTRUCTURAL ASPECTS OF FRACTURE ...
Other editions - View all
Common terms and phrases
addition alloy aluminum alloy applied stress associated ASTM atoms behavior brittle ceramics Chapter Charpy component composite crack extension crack growth crack length crack tip craze creep rate crystal curve cyclic decrease depends determined dislocation ductility elastic embrittlement engineering example factor failure fiber FIGURE flaw fracture mechanics fracture surface fracture toughness given grain boundaries hardening hydrogen increasing initial KIEAC lattice load maraging steels martensite material material's matrix Metals Park microstructure microvoid modulus notch Note occur oriented parameter particles phase plane plane-strain plastic deformation plastic zone plate polymer polymeric region relative Reprinted with permission result rupture sample screw dislocation Section shear stress shown in Fig solid solution specimen stacking fault energy steel alloys strain rate stress concentration stress field stress intensity stress level stress-strain stress-strain curve superalloys tensile stress test temperature thermal thickness toughening Trans transition temperature twinning values yield strength