Proceedings of the ... International Conference on Offshore Mechanics and Arctic Engineering, Volume 18, Part 3American Society of Mechanical Engineers, 2000 - Arctic regions |
From inside the book
Results 1-3 of 65
Page 26
... fracture toughness for use in defect assessment of safety critical components . This paper outlines the SINTAP mml procedure and illustrates it using fracture toughness obtained from a weld metal , HAZ and parent plate . Furthermore ...
... fracture toughness for use in defect assessment of safety critical components . This paper outlines the SINTAP mml procedure and illustrates it using fracture toughness obtained from a weld metal , HAZ and parent plate . Furthermore ...
Page 27
... fracture toughness distribution . The procedure described above can , in principle , be applied to data in the fracture toughness transition regime . In this case the temperature dependence of fracture toughness for ferritic steels is ...
... fracture toughness distribution . The procedure described above can , in principle , be applied to data in the fracture toughness transition regime . In this case the temperature dependence of fracture toughness for ferritic steels is ...
Page 263
... fracture toughness requirement of materials . A new concept , equivalent CTOD concept , is introduced on the basis of the Local Approach . The equivalent CTOD is defined by the CTOD of the fracture toughness specimen , at which the fracture ...
... fracture toughness requirement of materials . A new concept , equivalent CTOD concept , is introduced on the basis of the Local Approach . The equivalent CTOD is defined by the CTOD of the fracture toughness specimen , at which the fracture ...
Contents
STRUCTURAL INTEGRITY PROCEDURES FOR EUROPE SINTAP | 1 |
OMAE99MAT2041 | 9 |
Development of the SINTAP Failure Assessment Diagrams for Compatibility With | 19 |
Copyright | |
28 other sections not shown
Other editions - View all
Common terms and phrases
addition analysis applications approach ASME assessment base behavior bending CGHAZ Charpy compared component composite condition Conference Copyright crack critical CTOD curve defects deposition depth determined developed distribution dynamic effect element energy Engineering equations equivalent evaluated factors failure fatigue ferrite Figure fire fracture toughness function geometry given hardness heat input impact important improve increase initiation International joints length limit loading lower material matrix maximum mean measured mechanical method microstructure molten observed obtained offshore operating parameters performance phase pipe plate prediction present pressure procedure production properties protection range ratio reduced region requirements residual stress respectively risers safety ship shown shows specimens standards steel strain strength structures surface Table temperature tensile thickness values weld metal welded joints wire yield