... length and temperature . The peak wave length , which irradiates maximum strength and temperature of the material , are determined by Wien's law . Irradiated light itself has typical wave length distribution determined by temperature ...
... length and temperature . The peak wave length , which irradiates maximum strength and temperature of the material , are determined by Wien's law . Irradiated light itself has typical wave length distribution determined by temperature ...
Page 100
... length is about 30mm . The water around welding portion is also turbid by preparing operation such as cleaning and ... length between the plate surface and the window surface of the camera is 15mm . The actual length between the plate ...
... length is about 30mm . The water around welding portion is also turbid by preparing operation such as cleaning and ... length between the plate surface and the window surface of the camera is 15mm . The actual length between the plate ...
Page 101
... length in turbid water . The image quality was improved by this technique . Groove geometry can be evaluated up to transparency length of 25mm when the actual light path length is 30mm . The simple algorithm to evaluate root gap width ...
... length in turbid water . The image quality was improved by this technique . Groove geometry can be evaluated up to transparency length of 25mm when the actual light path length is 30mm . The simple algorithm to evaluate root gap width ...
Contents
STRUCTURAL INTEGRITY PROCEDURES FOR EUROPE SINTAP | 1 |
OMAE99MAT2041 | 9 |
Development of the SINTAP Failure Assessment Diagrams for Compatibility With | 19 |
Copyright | |
28 other sections not shown
Other editions - View all
Common terms and phrases
addition analysis applications approach ASME assessment base behavior bending CGHAZ Charpy compared component composite condition Conference Copyright crack critical CTOD curve defects deposition depth determined developed distribution dynamic effect element energy Engineering equations equivalent evaluated factors failure fatigue ferrite Figure fire fracture toughness function geometry given hardness heat input impact important improve increase initiation International joints length limit loading lower material matrix maximum mean measured mechanical method microstructure molten observed obtained offshore operating parameters performance phase pipe plate prediction present pressure procedure production properties protection range ratio reduced region requirements residual stress respectively risers safety ship shown shows specimens standards steel strain strength structures surface Table temperature tensile thickness values weld metal welded joints wire yield