Page 49
... pipe manufacturing industry over the last 15 years which have encompassed manufacturing techniques , chemical analyses of pipe plate , increases in thicknesses and strengths of pipe and developments in welding technology . These changes ...
... pipe manufacturing industry over the last 15 years which have encompassed manufacturing techniques , chemical analyses of pipe plate , increases in thicknesses and strengths of pipe and developments in welding technology . These changes ...
Page 52
... pipe mill environments for the welding of thin wall pipe giving consistent performance with low defect rates over a range of pipe wall thicknesses . SUMMARY The developments which have taken place in welding consumables for the multi ...
... pipe mill environments for the welding of thin wall pipe giving consistent performance with low defect rates over a range of pipe wall thicknesses . SUMMARY The developments which have taken place in welding consumables for the multi ...
Page 203
... PIPES The Norwegian pipe manufacturer NAT Compipe was recently awarded the world's first commercial contract for continuous spoolable composite pipes . The delivery is 16.3km ( 10.1 miles ) , 3 " , 380 bar Compipe pipe delivered in ...
... PIPES The Norwegian pipe manufacturer NAT Compipe was recently awarded the world's first commercial contract for continuous spoolable composite pipes . The delivery is 16.3km ( 10.1 miles ) , 3 " , 380 bar Compipe pipe delivered in ...
Contents
STRUCTURAL INTEGRITY PROCEDURES FOR EUROPE SINTAP | 1 |
OMAE99MAT2041 | 9 |
Development of the SINTAP Failure Assessment Diagrams for Compatibility With | 19 |
Copyright | |
28 other sections not shown
Other editions - View all
Common terms and phrases
addition analysis applications approach ASME assessment base behavior bending CGHAZ Charpy compared component composite condition Conference Copyright crack critical CTOD curve defects deposition depth determined developed distribution dynamic effect element energy Engineering equations equivalent evaluated factors failure fatigue ferrite Figure fire fracture toughness function geometry given hardness heat input impact important improve increase initiation International joints length limit loading lower material matrix maximum mean measured mechanical method microstructure molten observed obtained offshore operating parameters performance phase pipe plate prediction present pressure procedure production properties protection range ratio reduced region requirements residual stress respectively risers safety ship shown shows specimens standards steel strain strength structures surface Table temperature tensile thickness values weld metal welded joints wire yield