... specimens , respectively , to validate the formulations in equations ( 28 ) and ( 29 ) [ 14 ] . In the first series of tests , five pairs of centre - cracked plate specimens , where each pair consisted of one specimen containing ...
... specimens , respectively , to validate the formulations in equations ( 28 ) and ( 29 ) [ 14 ] . In the first series of tests , five pairs of centre - cracked plate specimens , where each pair consisted of one specimen containing ...
Page 119
... specimens were designed and contoured to minimize the risk of fatigue failures outside the weld area . The specimens were at least four thicknesses wide at the test weld section to minimize edge effects . Series Two series of eight ( 8 ) ...
... specimens were designed and contoured to minimize the risk of fatigue failures outside the weld area . The specimens were at least four thicknesses wide at the test weld section to minimize edge effects . Series Two series of eight ( 8 ) ...
Page 277
... specimens for both SMAW and SAW simulation , SMAW case was mainly analyzed in the following study . The fractographs of the tested specimens at 77K are shown in Fig . 4. From the figure , the UA CGHAZ specimens showed the transgranular ...
... specimens for both SMAW and SAW simulation , SMAW case was mainly analyzed in the following study . The fractographs of the tested specimens at 77K are shown in Fig . 4. From the figure , the UA CGHAZ specimens showed the transgranular ...
Contents
STRUCTURAL INTEGRITY PROCEDURES FOR EUROPE SINTAP | 1 |
OMAE99MAT2041 | 9 |
Development of the SINTAP Failure Assessment Diagrams for Compatibility With | 19 |
Copyright | |
28 other sections not shown
Other editions - View all
Common terms and phrases
absorbed energy analysis Arctic Engineering July ASME assessment austenite base metal behavior bending brace CGHAZ Charpy impact Charpy impact test chord component composite material Conference On Offshore copper backing Copyright CTOD value curve cyclic defects developed dynamic effect Engineering July 11-16 equations equivalent CTOD evaluated fatigue tests ferrite fiber fire flux fracture toughness geometry GMAW GTAW HAZ toughness heat input increase intumescents iteration matrix maximum mechanical properties Mechanics and Arctic method microstructure notch obtained Offshore Mechanics offshore structures parameters passive fire protection porosity procedure Proceedings of OMAE99 PWHT ratio requirements residual stress risers S-N curve SCFEX shielding gas short circuiting SINTAP specimens standards steel plates strain stress intensity submerged arc welding surface Table temperature test results thickness titanium underwater welding Weibull stress weld metal weld pool weld toe welded joints wet welding wide plate wire yield strength