Proceedings of the ... International Conference on Offshore Mechanics and Arctic Engineering, Volume 14, Part 3American Society of Mechanical Engineers, 1995 - Arctic regions |
From inside the book
Results 1-3 of 84
Page 38
Table 9 shows that the scatter , represented by the ratio of the mean to design life , is greater for the results based ... The comparison of predictions of SCF from the parametric equations and from FE analyses for five leg joints show ...
Table 9 shows that the scatter , represented by the ratio of the mean to design life , is greater for the results based ... The comparison of predictions of SCF from the parametric equations and from FE analyses for five leg joints show ...
Page 359
Figure 3 shows the schematic diagram of thermal history and deformation patterns and their obtained microstructures . Ferrite in the heating process can be deformed at temperature which is high enough for the defomed ferrite to be ...
Figure 3 shows the schematic diagram of thermal history and deformation patterns and their obtained microstructures . Ferrite in the heating process can be deformed at temperature which is high enough for the defomed ferrite to be ...
Page 548
The reference effective sound pressure shows a minimum pressure change which human beings can recognize in normal frequency range . Ale Microphone -2.5m > Data recorder Test plate 1.5m Microphone Only an alternative pressure change is ...
The reference effective sound pressure shows a minimum pressure change which human beings can recognize in normal frequency range . Ale Microphone -2.5m > Data recorder Test plate 1.5m Microphone Only an alternative pressure change is ...
What people are saying - Write a review
We haven't found any reviews in the usual places.
Contents
FATIGUE GUIDANCE FOR OFFSHORE STRUCTURES | 16 |
VOLUME IA OFFSHORE TECHNOLOGY VOLUME II MATERIALS ENGINEERING | 18 |
VOLUME 1B OFFSHORE TECHNOLOGY VOLUME IV ARCTICPOLAR TECHNOLOGY | 135 |
Copyright | |
15 other sections not shown
Other editions - View all
Common terms and phrases
analysis applied approach assessment behaviour bending brace calculated carried chord compared comparison concentration connections crack growth crack tip CTOD curve cycles defect depth determined developed distribution effect Engineering equations estimated evaluation experimental factor failure fatigue crack Figure finite element fracture geometry given guidance heating higher improved included increase influence initiation International length limit load lower material mean measured Mechanics method microstructure mode notch obtained Offshore parameters performed pipe plastic plate position predictions present procedure properties range ratio reduced region repair Report Research residual stress shape shown shows side specimens steel strain strength stress intensity factor structures surface Table temperature tensile thickness toughness tubular joints values weld metal weld toe welded joints wide yield yield strength