C 1995 OMAE - Volume III , Materials Engineering ASME 1995 ABSTRACT The effect of yield strength mismatch on the behaviour of semielliptical surface cracks , with alt = 0.25 and a / c = 0.25 , located in weld metal has been investigated ...
C 1995 OMAE - Volume III , Materials Engineering ASME 1995 ABSTRACT The effect of yield strength mismatch on the behaviour of semielliptical surface cracks , with alt = 0.25 and a / c = 0.25 , located in weld metal has been investigated ...
Page 272
Finally , to provide guidelines for the way forward , work in progress at Cranfield and elsewhere is discussed to try to resolve some of the current issues . to the lesser value of the yield strength or UTS ( 0.7 in the UK ) P : 24,23 ...
Finally , to provide guidelines for the way forward , work in progress at Cranfield and elsewhere is discussed to try to resolve some of the current issues . to the lesser value of the yield strength or UTS ( 0.7 in the UK ) P : 24,23 ...
Page 367
Indeed , preliminary studies on simple joints indicate that steels higher strength levels and with higher yield ... in tems of load redistribution and yielding , and enable significant increases in joint load capacity to be achieved .
Indeed , preliminary studies on simple joints indicate that steels higher strength levels and with higher yield ... in tems of load redistribution and yielding , and enable significant increases in joint load capacity to be achieved .
What people are saying - Write a review
We haven't found any reviews in the usual places.
Contents
FATIGUE GUIDANCE FOR OFFSHORE STRUCTURES | 16 |
VOLUME IA OFFSHORE TECHNOLOGY VOLUME II MATERIALS ENGINEERING | 18 |
VOLUME 1B OFFSHORE TECHNOLOGY VOLUME IV ARCTICPOLAR TECHNOLOGY | 135 |
Copyright | |
15 other sections not shown
Other editions - View all
Common terms and phrases
analysis applied approach assessment behaviour bending brace calculated carried chord compared comparison concentration connections crack growth crack tip CTOD curve cycles defect depth determined developed distribution effect Engineering equations estimated evaluation experimental factor failure fatigue crack Figure finite element fracture geometry given guidance heating higher improved included increase influence initiation International length limit load lower material mean measured Mechanics method microstructure mode notch obtained Offshore parameters performed pipe plastic plate position predictions present procedure properties range ratio reduced region repair Report Research residual stress shape shown shows side specimens steel strain strength stress intensity factor structures surface Table temperature tensile thickness toughness tubular joints values weld metal weld toe welded joints wide yield yield strength