Proceedings of the ... International Conference on Offshore Mechanics and Arctic Engineering, Volume 3American Society of Mechanical Engineers, 2001 - Arctic regions |
From inside the book
Results 1-3 of 93
Page 174
MALNVVV Pretreatment of hot metal Quarter thickness Mid thickness LD
converter Secondary refining Continuous casting Reheating Rolling ( 63 . 5mm
thick . ) Accelerated cooling Figure 8 Manufacturing processes of developed steel
plates ...
MALNVVV Pretreatment of hot metal Quarter thickness Mid thickness LD
converter Secondary refining Continuous casting Reheating Rolling ( 63 . 5mm
thick . ) Accelerated cooling Figure 8 Manufacturing processes of developed steel
plates ...
Page 179
produced by ice ' s crushing again vertical structures , which has the following
form : F . = 1fO , DH ( 8 ) where , F is ice force , KN ; Oc is crushing strength of sea
ice , MPa ; H is ice thickness , cm ; d is diameter or width of structural member ...
produced by ice ' s crushing again vertical structures , which has the following
form : F . = 1fO , DH ( 8 ) where , F is ice force , KN ; Oc is crushing strength of sea
ice , MPa ; H is ice thickness , cm ; d is diameter or width of structural member ...
Page 196
First , the thickness difference between CTOD specimens and CCA specimens
due to the side grooves in CCA test specimens should be corrected because
fracture toughness increases with decreasing thickness . Japanese standard ...
First , the thickness difference between CTOD specimens and CCA specimens
due to the side grooves in CCA test specimens should be corrected because
fracture toughness increases with decreasing thickness . Japanese standard ...
What people are saying - Write a review
We haven't found any reviews in the usual places.
Contents
OMAE2001MAT3010 | 1 |
OMAE2001MAT3011 | 11 |
OMAE2001MAT3013 | 17 |
Copyright | |
45 other sections not shown
Other editions - View all
Common terms and phrases
analysis applied assessment bending boundary buckling calculated Charpy compared components compressive considered controlled corrosion crack crack initiation critical CTOD curve cycle defects defined deformation derivatives determined developed direction discrete displacement distribution ductile crack dynamic effect element Engineering equation estimated evaluated experiments factors failure fatigue fatigue cracks field Figure finite element flexible FPSO fracture toughness function geometry grain growth higher impact increase inspection International joints layer length loading material maximum measured mechanical metal method microstructure node notch observed obtained offshore operation parameters performed phase pipe pipeline plastic plate predicted present pressure prestrained problem procedure range region respectively riser shown shows simulated specimens standard steel strain strength stress structures surface Table technique temperature tensile thickness weight weld yield