Encyclopedia of Physical Science and Technology, Volume 19Robert A. Meyers The Encyclopedia of Physical Science and Technology contains in-depth presentations on all of today's critical technology areas, including: Materials synthesis and processing Electronic and photonic materials synthesis and processing Electronic and photonic materials Ceramics Composites High performance metals and alloys Flexible computer-integrated manufacturing Intelligent process equipment Micro- and nano-fabrication Software Microelectronics and opto-electronics High performance computing and networking High definition imaging and displays Sensors and signal processing Data storage and peripherals Computer simulation and modeling Aeronautics Surface transportation technologies Energy technologies Pollution remediation and waste management These technologies were specified as critical by a thirteen-member National Critical Technologies panel composed of government and private-sector members and chaired by chemist William D. Phillips. The Encyclopedia of Physical Science and Technology contains in-depth first-principle and applications descriptions of all the major emerging technologies in the physical sciences, inlcluding: Advanced materials Advanced semiconductor devices Artificial intelligence Digital imaging technology Flexible computer-integrated manufacturing High-density data storage High-performance computing Opto-electronics Sensor technology Superconductors The completely revised and updated Second Edition includes the following contributions: Thirty-one from the University of California that cover subjects ranging from nuclear energy, materials, mathematics, astronomy, and computers to anti-ballistic missile defense systems and laser applications Eighteen from the AT&T Bell Laboratories that cover communications disciplines, such as digital speech processing, telecommunications switching, and optical fibers Eleven from NASA that cover astronomy, atmospheric sciences, and space flight Nine from the University of Illinois that cover subjects ranging from manufacturing process technology and scientific information services to environmental data acquisition and very large scale integration (VLSI design) Eight from United States Navy Research Centers that cover x-ray lasers and telecommunications through non-linear optics and fluid dynamics Eight from the California Institute of Technology that cover astronomy, space sciences, and parallel computing Eight from the University of Colorado that cover subjects ranging from atomic physics ad geochemistry to telecommunications and the materials for microcircuitry Seven from the Electric Power Research Institute that cover power generation systems and air pollution Six from Cornell University that cover the solar system, bioprocess engineering, lasers, and dynamics Countries participating in the preparation of the Encyclopedia include: 76% United States institutions and 24% foreign institutions 12% with the European Economic Community (EEC)--7% of the contributors are from the United Kingdom, 3% are from Germany, and 1% are from Austria 1% Israel, France, and Japan 7% at institutions in Canada--the combination of the United States and Canada accounts for 83% of the contributions The author-institution community includes contributions from a total of eighteen countries--the United States, the United Kingdom, Canada, Germany, France, Israel, Japan, Austria, EEC institutions, Australia, Spain, the Netherlands, India, Korea, New Zealand, Sweden, Switzerland, and Italy The number of articles contributed by each country (excluding the United States) are: 49--the United Kingdom 46--Canada 22--Germany 9--France 7--Israel 7--Japan 5--Austria 2--EEC institutions 2--Australia 2--Spain 2--Netherlands 1--India 1--Korea 1--Norway 1--New Zealand 1--Sweden 1--Switzerland 1--Italy SUBJECT |
From inside the book
Results 1-3 of 8
Page 98
... Stress corrosion cracking of titanium tanks by N2O4 is inhibited by the addition of about 1 wt . % nitric oxide ( NO ) , the resulting formulation being called MON - 1 . To assure that there will always be sufficient NO for protection ...
... Stress corrosion cracking of titanium tanks by N2O4 is inhibited by the addition of about 1 wt . % nitric oxide ( NO ) , the resulting formulation being called MON - 1 . To assure that there will always be sufficient NO for protection ...
Page 118
... stress corrosion protection . Neat N2O4 ( NTO ) was used in the Titan II missile . MONS with the higher levels of NO will have higher vapor pressure . Otherwise , the safety , material compatibility , and handling characteris- tics for ...
... stress corrosion protection . Neat N2O4 ( NTO ) was used in the Titan II missile . MONS with the higher levels of NO will have higher vapor pressure . Otherwise , the safety , material compatibility , and handling characteris- tics for ...
Page 569
... stress that results in shortening . Creep : Time and temperature dependent de- formation . Dead load : Weight of the ... corrosion : stress . Corrosion accelerated by Structure : Load - carrying part of a building , a bridge , or an ...
... stress that results in shortening . Creep : Time and temperature dependent de- formation . Dead load : Weight of the ... corrosion : stress . Corrosion accelerated by Structure : Load - carrying part of a building , a bridge , or an ...
Contents
Liquid Chromatography 13 Main Group Elements 363 Russell L Rasmussen Joseph | 39 |
Liquid Crystal Devices 41 Manifold Geometry 397 | 39 |
Michael G Clark | 41 |
Copyright | |
20 other sections not shown
Other editions - View all
Common terms and phrases
acid alkali metals applications atoms bond brane carbon cell chain chemical chromatography column components composition compounds concentration core defined density detector device electric electrons elements emission energy engine equation example excited ferromagnetic finite flow fluorine flux force frequency fuel function gradient heat HPLC hydrazine hydrogen integral isotactic layer liquid alkali metals liquid crystal LISP lithium load machine magnetic field mantle masonry materials measure melting membrane method mobile phase molecular molecules monomer nematic nitrogen oxide oxygen packing particles polar polymer pressure propellant properties protons pump reaction result reverse osmosis rotation sample Section separation sequence shown in Fig silica smectic sodium solid solution solvent space specific spin stress structure surface syndiotactic temperature theorem theory thermal tion tool ture units vector velocity viscosity voltage workpiece