Proceedings of the ... International Conference on Offshore Mechanics and Arctic Engineering, Volume 10American Society of Mechanical Engineers, 1991 - Arctic regions |
From inside the book
Results 1-3 of 75
Page 164
... reduced time consumption , and the resulting motivation factors for using the technology can now be summarized as follows : * Reduced costs for qualifying procedures and personnel . Lower costs for diving personnel . Improved weld ...
... reduced time consumption , and the resulting motivation factors for using the technology can now be summarized as follows : * Reduced costs for qualifying procedures and personnel . Lower costs for diving personnel . Improved weld ...
Page 252
... reduced welding in deck - Up to 60 % reduced welding in the walls - - - - No painting is strictly required No welding of hanger support points under deck No floor screed No turning operation of each deck Most weld bevels included in ...
... reduced welding in deck - Up to 60 % reduced welding in the walls - - - - No painting is strictly required No welding of hanger support points under deck No floor screed No turning operation of each deck Most weld bevels included in ...
Page 282
... reduction , and 3 ) reduced life cycle costs derived from improved corrosion resistance and reliability with reduced downtime / maintenance costs . Therefore , titanium alloys can become even more cost attractive in certain weight ...
... reduction , and 3 ) reduced life cycle costs derived from improved corrosion resistance and reliability with reduced downtime / maintenance costs . Therefore , titanium alloys can become even more cost attractive in certain weight ...
Contents
RESIDUAL STRESS AND DISTORTION IN WELDS | 1 |
WELD METAL AND HAZ PROPERTIES | 37 |
The Effect of Intercritical Thermal Cycles on HAZ Microstructure and Toughness in CMnAlNb | 49 |
Copyright | |
17 other sections not shown
Other editions - View all
Common terms and phrases
aluminium austenite axial base metal bead behaviour brittle CGHAZ Charpy Charpy impact test chemical composition coating cooling corrosion crack front crack tip critical CTOD CTOD fracture toughness CTOD test CTOD value deformation developed distribution effect energy evaluation experimental fatigue crack ferrite Figure gauges Grade grain coarsened HAZ groove HAZ toughness heat input hydrogen cracking ICCGHAZ inherent strain intercritical kJ/mm load martensite Materials Engineering ASME measured mechanical properties method microstructure narrow gap notched panel obtained OMAE peak temperature pearlite pipe pipeline Pop-in pressure PWHT reheated residual stress samples seawater shielding gas simulation single-U Statoil steel plates steel TM1 strain gauges submerged arc welding surface notched specimen Table tempered tensile strength thermal cycle through-thickness notched TMCP steels underwater welding Volume III-A weld metal weldability welded joint welding conditions Welding Institute welding parameters welding procedure welding process welding residual stress weldment width yield strength