Page 71
“Durichlor”, “Duriron”, and “Corrosiron” are not recommended for mixtures of
chlorine and steam or mixtures of hydrogen, chlorine, and steam. None of the
silicon cast irons has useful resistance to hydrofluoric acid, fluoride salts,
sulfurous acid, ...
“Durichlor”, “Duriron”, and “Corrosiron” are not recommended for mixtures of
chlorine and steam or mixtures of hydrogen, chlorine, and steam. None of the
silicon cast irons has useful resistance to hydrofluoric acid, fluoride salts,
sulfurous acid, ...
Page 114
Carbide-tipped tools are not mandatory but are recommended in preference to
the high speed tool steels. The tool should not ride the work as it causes work-
hardening of the surface. When properly machined, the surface has a better
surface ...
Carbide-tipped tools are not mandatory but are recommended in preference to
the high speed tool steels. The tool should not ride the work as it causes work-
hardening of the surface. When properly machined, the surface has a better
surface ...
Page 277
In spite of the need for compounding on the jobsite and the necessity for a
sandblasted surface, the epoxies are proving themselves to be of great value to
the process industries. While these coatings are not generally recommended for
...
In spite of the need for compounding on the jobsite and the necessity for a
sandblasted surface, the epoxies are proving themselves to be of great value to
the process industries. While these coatings are not generally recommended for
...
What people are saying - Write a review
We haven't found any reviews in the usual places.
Other editions - View all
Common terms and phrases
abrasion acid addition alkalies alloys aluminum annealed anode applications atmospheres attack austenitic base brasses carbon carbon steel cast iron cause cements cent characteristics chemical resistance chloride cleaning coat combination COMPANY compounds concentrations conductivity construction containing continuous cooling copper corrosion corrosion resistance cost cracking ductility effect electrical elevated Elongation environments equipment excellent exposure fabrication film given grades gray greater handled hardness heat heat-treatment impact improved increase industries lead limited lining lower machining material maximum mechanical properties metal method Monel natural nickel nitric normally occurs operating organic oxidizing paint performed physical pipe plastic prevent protection range readily recommended reducing removed rubber salts silicon sodium hypochlorite solutions solvents stainless steels stress structure suitable sulfuric acid superior surface Table temperature tensile strength thermal tion titanium Type Typical welding widely wrought zinc