Page 107
... thickness crack . The number of cycles to the end of the test as defined by joint separation or a specified crack length or a specified loss of specimen stiffness . The values of N1 and N2 reflect fatigue crack initiation and small ...
... thickness crack . The number of cycles to the end of the test as defined by joint separation or a specified crack length or a specified loss of specimen stiffness . The values of N1 and N2 reflect fatigue crack initiation and small ...
Page 93
WALL THICKNESS DESIGN FOR HIGH PRESSURE OFFSHORE GAS PIPELINES Richard Verley , Sverre Lund , and Hermann Moshagen Statoil Stavanger , Norway Gresnigt , A.M. , 1986 , " Plastic design of. 1994 OMAE - Volume V , Pipeline Technology ASME ...
WALL THICKNESS DESIGN FOR HIGH PRESSURE OFFSHORE GAS PIPELINES Richard Verley , Sverre Lund , and Hermann Moshagen Statoil Stavanger , Norway Gresnigt , A.M. , 1986 , " Plastic design of. 1994 OMAE - Volume V , Pipeline Technology ASME ...
Page 97
... thickness tolerances . The newer design Codes , e.g. BS 8010 part 3 , give considerably lower true stress levels than the traditional design ( for D / t > 20 , by a percentage corresponding to the wall thickness negative tolerance in ...
... thickness tolerances . The newer design Codes , e.g. BS 8010 part 3 , give considerably lower true stress levels than the traditional design ( for D / t > 20 , by a percentage corresponding to the wall thickness negative tolerance in ...
Contents
FATIGUE AND DEFORMATION | 1 |
FRACTURE ASSESSMENT AND ANALYSIS | 37 |
FATIGUE DESIGN AND DETECTION | 73 |
Copyright | |
29 other sections not shown
Other editions - View all
Common terms and phrases
analysis angle applied ASME assessment axial behaviour bending calculated cathodic protection corrosion crack growth rate crack propagation crack tip CTOD cycles deformation developed diameter displacement drillpipe dynamic elastic equation experimental factor failure fatigue crack growth fatigue strength ferrite finite element fracture mechanics fracture toughness free span geometry heat hoop stress hydrogen Ice Class increase initial installation J-Lay length limit load material maximum mbar method microstructure modulus nitrogen notch obtained offshore structures OMAE operating parameters pipe pipeline plastic Poisson's ratio predicted pressure ratio repair residual stress S-N curve scour sea ice sea water shielding gas simulated soil sour crude oil specimens steel strain rate stress intensity stress range surface Table Technology temperature tensile tubular joints values wall thickness water depth weld deposit weld metal weld toe weldment size effect wire yield strength Young's modulus