Alloy Modeling & Design: Proceedings of a Symposium Sponsored by the TMS Structural Materials Division (SMD), the Committee on Alloy Phases (CAP), and the Electronic, Magnetic and Photonic Materials Division (EMPMD), the Oak Ridge National Laboratory and the Lawrence Livermore National Laboratory, Held During Materials Week '93, Pittsburgh, Pennsylvania, October 18-20, 1993G. M. Stocks, Patrice E. A. Turchi This work brings together contributions from researchers in a variety of fields that have a common interest in applying the most recent developments in basic research to the design of new alloys. The papers are from Materials Week '93 held in Pittsburgh, Pennsylvania, October 17-21, 1993. |
From inside the book
Results 1-3 of 4
Page 310
... substrate , is that the growth mode is of the Frank van der Merwe ( FM ) type , i.e. a layer - by - layer growing mode . This FM growth implies that the first A monolayer wets the substrate , i.e. , in a simplified macroscopic ...
... substrate , is that the growth mode is of the Frank van der Merwe ( FM ) type , i.e. a layer - by - layer growing mode . This FM growth implies that the first A monolayer wets the substrate , i.e. , in a simplified macroscopic ...
Page 311
... substrate like for example bcc Co / bcc Fe or Cr , fcc Co / fcc Cu or Pd , fcc Fe / fcc Cu or Ir , bcc Ni / bcc Fe . A discrepancy holds for Co / Cu ( 100 ) between Schuster et al . [ 7 ] who identify by LEED and MEED a bct Co structure ...
... substrate like for example bcc Co / bcc Fe or Cr , fcc Co / fcc Cu or Pd , fcc Fe / fcc Cu or Ir , bcc Ni / bcc Fe . A discrepancy holds for Co / Cu ( 100 ) between Schuster et al . [ 7 ] who identify by LEED and MEED a bct Co structure ...
Page 317
... substrates . The critical thickness of the metastable structure is limited to some monolayers and it is slightly dependent on the lattice mismatch with the substrate . The critical thickness is generally increased in multilayers ( 5 to ...
... substrates . The critical thickness of the metastable structure is limited to some monolayers and it is slightly dependent on the lattice mismatch with the substrate . The critical thickness is generally increased in multilayers ( 5 to ...
Contents
CONSEQUENCES OF OSCILLATORY POTENTIALS AND ANGULAR | 13 |
FIRSTPRINCIPLES TIGHTBINDING TOTAL ENERGY | 25 |
Contributed Papers | 33 |
Copyright | |
30 other sections not shown
Common terms and phrases
10Ti alloy Acta Metall Al-Li Alloy Modeling Alloy Phase alloys annealing APB energy approximation atom probe behavior binary alloys cluster expansion composition computed configuration density Design Edited dislocation displacement ductility Edited by G.M. effect elastic constants electronic structure entropy equivolume expansion experimental FeAl Fermi energy Fermi surface Figure first-principles formation energy free energy friction stress G.M. Stocks glide plane grain boundaries Grand Potential Hamiltonian increase intermetallic compounds Ising model lattice constants lattice parameter Lett magnetic Materials Science Materials Society matrix measured Metals & Materials method Modeling and Design nearest neighbor Ni3Al NiAl obtained ordered P.E.A. Turchi phase diagram phase stability phonon Phys plane point defects potential predicted samples screw shown in Fig simulations solid solution Stocks and P.E.A. stoichiometry sublattice techniques ternary theory thermal tight-binding total energy transition metal trialuminides Turchi The Minerals unit cell vibrational x-ray
References to this book
Encyclopedia of Applied Physics, Volume 18 George L. Trigg,Eduardo S. Vera,Walter Greulich No preview available - 1997 |